Composition for fireproof material, manufacturing method thereof and its usage 发明申请

2022-07-31 2870 38K 0

专利信息

申请日期 2024-11-18 申请号 KR1020030039785
公开(公告)号 KR1020040110453A 公开(公告)日 2004-12-31
公开国别 KR 申请人省市代码 全国
申请人 KOREA INSTITUTE OF CERAMIC ENGINEERING TECHNOLOGY; NECES SARY CO LTD
简介 PURPOSE : A composition of a fireproof material is provided to improve water resistance, heat insulation and fire proofing property, and to lighten the weight, thereby being suitably used as an interior material for a fireproof door. CONSTITUTION : The composition of a fireproof material comprises 40-95wt% of light inorganic fine particles; 2.5-50wt% of an inorganic binder in liquid phase; and 5-50wt% of alumina cement, wherein the light fine particles is selected from at least one of pearlite, vermiculite, diatomaceous earth and activated carbon, which have a particle size of 0.1-10mm. The composition of a fireproof material is produced by mixing the above-mentioned components with above-mentioned ratio, and carrying out compress molding the mixture with 0.1-1kgf/cm2 of pressure at 200-250deg.C. © KIPO 2005


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报