For the anisotropic magnetic powder secondary particle and production of anisotropic magnetic powder 发明授权

2022-07-07 3700 133K 0

专利信息

申请日期 2025-04-23 申请号 JP2018091445
公开(公告)号 JP6447768B2 公开(公告)日 2019-01-09
公开国别 JP 申请人省市代码 全国
申请人 日亜化学工業株式会社
简介 Provided are a method of producing a titanium-containing rare earth-iron-nitrogen anisotropic magnetic powder having good magnetic properties, and secondary particles for a titanium-containing anisotropic magnetic powder. The method includes : obtaining a first precipitate containing R, iron, and titanium by mixing a first precipitating agent with a solution containing R, iron, and titanium, wherein R is at least one selected from Sc, Y, Pr, Nd, Pm, Sm, Gd, Tb, Dy, Ho, Er, Tm, and Lu; obtaining a second precipitate containing R and iron by mixing, in the presence of the first precipitate, a second precipitating agent with a solution containing R and iron; obtaining an oxide containing R, iron, and titanium by calcining the second precipitate; obtaining a partial oxide by heat treating the oxide in a reducing gas atmosphere; obtaining alloy particles by reducing the partial oxide; and obtaining an anisotropic magnetic powder by nitriding the alloy particles.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报