METHOD FOR EXTRACTION, ENRICHMENT AND RECOVERY OF RARE EARTHS FROM LOW-CONCENTRATION RARE EARTH SOL 发明申请

2022-06-06 4570 1686K 0

专利信息

申请日期 2025-02-22 申请号 WOCN17096222
公开(公告)号 WO2018028543A1 公开(公告)日 2018-02-15
公开国别 WO 申请人省市代码 全国
申请人 GRIREM ADVANCED MATERIALS CO LTD
简介 A method for extraction, enrichment and recovery of rare earths from a low-concentration rare earth solution, using a non-saponification organic extractant to perform centrifugal extraction, obtaining an organic phase containing rare earths and a raffinate; using an inorganic acid to perform centrifugal back-extraction on the organic phase containing rare earths, obtaining a rare earth enriched liquid. Low-concentration rare earth solution indicates a rare earth solution having REO concentration of 0.05-8g/L. Single or dual coupled centrifugal extraction is performed, at an extraction mixing time of 5-60s. The present method has simple operation, protects the environment, and has a high rare earth recovery rate.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报