客服热线:18202992950

Optical glass, hot molding and its manufacturing method, and an optical element and manufacturing 发明授权

2022-06-06 3320 1569K 0

专利信息

申请日期 2025-02-27 申请号 JP2014560805
公开(公告)号 JP6338537B2 公开(公告)日 2018-06-06
公开国别 JP 申请人省市代码 全国
申请人 HOYA株式会社
简介 An optical glass includes P2O5, B2O3 and a rare earth oxide as essential components, and in a glass composition based on oxides, the P2O5 content is in the range of over 0 weight % and less than 0.79 weight %, the B2O3 content is in the range of 20-40 weight % and the total content of the rare earth oxide and an oxide selected from the group including of Ta2O5, WO3, TiO2, Nb2O5 and Bi2O3 is in the range of 35-70 weight %. Further, this optical glass has a refractive index (nd) in the range of 1.72-1.83, an Abbe number (υd) in the range of 45-55 and a glass transition temperature (Tg) of 640° C. or less.